The invention discloses a preparation method of micron-sized titanium dioxide, and relates to the technical field of coatings. The invention discloses a preparation method of micron-sized titanium dioxide, which comprises the following preparation steps: (1) pretreatment of raw materials: grinding and sieving the titanium dioxide raw materials to obtain pretreated raw materials; (2) acidolysis: putting the pretreated raw materials into sulfuric acid, stirring, filtering, and collecting filtrate; (3) hydrolysis: adding water into the filtrate for dilution, then adding a sodium hydroxide solution for mixing and stirring, heating for the first time, preserving heat, heating for the second time, adding a self-made magnetic flocculant, stirring, standing, fishing out, cooling to a proper temperature, adding an initiator, continuously stirring, standing, concentrating, filtering, and taking filter residues; (4) calcining: washing the filter residue with deionized water until the washed deionized ...