26-04-2018 дата публикации
Номер: WO2018074887A1
Принадлежит:
A method for manufacturing a high-strength reinforcing steel according to an embodiment comprises: a step for re-heating a slab at a temperature range of 1000-1100°C, the slab comprising, by means of wt%, 0.18-0.45% of carbon (C), 0.05-0.30% of silicon (Si), 0.40-3.00% of manganese (Mn), more than 0 and equal to or less than 0.04% of phosphorus (P), more than 0 and equal to or less than 0.04% of sulfur (S), more than 0 and equal to or less than 1.0% of chromium (Cr), more than 0 and equal to or less than 0.50% of copper (Cu), more than 0 and equal to or less than 0.25% of nickel (Ni), more than 0 and equal to or less than 0.50% of molybdenum (Mo), more than 0 and equal to or less than 0.040% of aluminum (Al), more than 0 and equal to or less than 0.20% of vanadium (V), more than 0 and equal to or less than 0.040% of nitrogen (N), more than 0 and equal to or less than 0.1% of antimony (Sb), more than 0 and equal to or less than 0.1% of tin (Sn), and the balance iron (Fe) and other inevitably ...
Подробнее