The invention discloses a manufacturing method of a hypereutectic high-chromium cast iron screw. Comprising the following steps: (1) smelting in an intermediate frequency furnace: charging materials are high-quality scrap steel, high-purity pig iron, low-phosphorus alloyed iron alloy or industrial pure metal, and P in molten iron is less than or equal to 0.015%; reducing slag is produced in the furnace. (2) casting ladle molten iron treatment: the tapping temperature is gt; and inert gas is fed into the ladle bottom to stir molten iron, wire feeding modification inoculation treatment is adopted, S in the molten iron is smaller than or equal to 0.010%, and O in the molten iron is smaller than or equal to 25 ppm. And (3) pouring is conducted, specifically, slag stopping and fixed-point pouring are conducted on a pouring ladle on a fixed-point pouring vehicle, whole-course CO2 or N2 protection is conducted through a top cap, a pouring chute and a pouring cup cover, modification inoculation ...