A press hardening steel by a medium and thin slab casting and direct rolling has a tensile strength 1900 MPa or more. The press hardening steel includes following chemical components by weight percent: C: 0.31-0.40%, Si: 0.36-0.44%, Mn: 1.6-2.0%, P≤0.006%, S≤0.004%, Als: 0.015-0.060%, Cr: 0.36-0.49%, Ti: 0.036-0.045% or Nb: 0.036-0.045% or V: 0.036-0.045%, or a mixture of the above two or more in any ratio, B: 0.004-0.005%, Mo: 0.26-0.35%, Ni: 0.11-0.20%, and N≤0.005%. A method for producing the press hardening steel includes following steps: desulphurizing molten iron; electric furnace or converter smelting and refining; continuous casting; descaling treatment before entering a soaking furnace; heating and soaking; high-pressure water descaling before entering a rolling mill; hot rolling; cooling; coiling; austenitizing; die deforming and quenching. 1. A press hardening steel , produced by a medium and thin slab casting and direct rolling and having a tensile strength 1900 MPa or more , the press hardening steel comprising following components by weight percent: C: 0.31%-0.40% , Si: 0.36%-0.44% , Mn: 1.6%-2.0% , P≤0.006% , S≤0.004% , Als: 0.015%-0.060% , Cr: 0.36%-0.49% , Ti: 0.036%-0.045% or Nb: 0.036%-0.045% or V: 0.036%-0.045% , or a mixture of the above two or more in any ratio , B: 0.004%-0.005% , Mo: 0.26%-0.35% , Ni: 0.11%-0.20% , N≤0.005% , and a balance of Fe and inevitable impurities , wherein a quenched microstructure is a full lath martensite; and mechanical properties are that a yield strength is larger than or equal to 1300 MPa , a tensile strength is larger than or equal to 1900 MPa , and elongation Ais larger than or equal to 5%.2. A method for producing the press hardening steel according to claim 1 , wherein the method comprising following steps:1) desulphurizing molten iron, and controlling S to be smaller or equal to 0.002%, an exposed surface of the molten iron after slagging off being not lower than 96%;2) performing conventional electric ...
Подробнее