The invention discloses a rare earth permanent ferrite material and a preparation method for devices made of same. The rare earth substituted permanent ferrite material has a hexagonal system, and has the chemical structural formula of A1-xRx.nFe2-y-zLnz/nCoy/nO3, wherein x is more than or equal to 0 and less than or equal to 0.8; y is more than or equal to 0 and less than or equal to 2.0; z is more than or equal to 0 and less than or equal to 3.0; n is more than or equal to 5.0 and less than or equal to 6.1; (1-x) is more than or equal to 0.2 and less than or equal to 1.0; A is one, two or three of Ca, Ba and Sr; R is one, two or three of chemical elements of La, Ce, Pr and Nd; and Ln is one, two or three of Sm, Eu, Gd, Dy, Ho, Er, Tm, Yb and Lu. Compared with the traditional permanent ferrite (AB12O19), the permanent ferrite material has the advantages that: the La, Ce, Pr and Nd in lanthanide rare earth partially replace ions at a position A, and the Sm, Eu, Gd, Dy, Ho, Er, Tm, Yb and ...