23-06-2023 дата публикации
Номер: CN116283276A
Принадлежит:
The chemical formula of the ferroelectric film material is Bi (4-x) LaxTi (3-y) SnyO12, x is more than 0 and less than or equal to 1, and y is more than 0 and less than or equal to 0.1. The preparation method comprises the steps of sol preparation, precursor film preparation, rapid heat treatment and ferroelectric film preparation. According to the method, bismuth nitrate hydrate, tin nitrate, lanthanum nitrate hydrate and tetrabutyl titanate are taken as precursors, citric acid is taken as a solvent, EDTA (Ethylene Diamine Tetraacetic Acid) is taken as a chelating agent to prepare a precursor solution, and the smooth and compact Bi (4-x) LaxTi (3-y) SnyO12 film is prepared through rapid heat treatment after spin coating. Compared with Bi4Ti3O12 and Bi4-xLaxTi3O12 films, the film has the advantages that the ferroelectric remanent polarization value and the anti-fatigue performance are remarkably improved, the preparation process of the film is simple, and expensive transition metal organic ...
Подробнее