The invention provides a technology for internal surface small space protection in an air flue of a dry-type air-core reactor. According to the technology for internal surface small space protection in the air flue of the dry-type air-core reactor, the inner surface of the air flue of the dry-type air-core reactor is processed. The technology comprises the following steps that dust in small space of the inner surface of the air flue of the air-core reactor is removed through a dust collection device, the bottom of the cleaned air flue of the air-core reactor is plugged through a plugging device, and therefore the air flue of the air-core reactor becomes a semi-closed container; paint is injected into the air flue of the air-core reactor, the air flue of the air-core reactor in the step (b) is dipped and coated, standing of the paint in the air flue of the air-core reactor is conducted for a period, the plugging device at the bottom of the air flue of the air-core reactor is detached after the paint is recycled, and quality detection is conducted on the treated air flue of the air-core reactor. According to the air-core reactor protected through the technology, the probability that due to the fact that water vapor molecules permeate through the air-core reactor, short circuits among wire turns of the air-core reactor are caused and then the air-core reactor is damaged is greatly reduced, and the service life of the air-core reactor is prolonged.

[1]



1. A dry-type hollow reactor passage inner surface of the process for protecting a small space, characterized in that the process comprises the following steps:

A, dust-removing device for the inner surface of the reactor air, remove the dust in the small space;

B, the plugging device of the step (a) of the clean air in the plugging at the bottom of the reactor, so that the reactor passage become a semi-closed container;

C, the air injected into the coating reactor, dip-coating the above-mentioned step (b) in the air passage of the reactor;

D, the coating in the reactor for a period of time in the air, so that the reactor passage surface for the thickness of the coating layer;

E, through the recovery apparatus for the coating of the reactor within an airway recovery processing;

F, the plugging device of the reactor at the bottom of the air passage;

G, through artificial appearance inspection tester for air coupling film thickness on the inner surface of the reactor after dip coating quality inspection, processing to the sagging phenomenon, to achieve uniform coating, the quality requirements of the formation.

2. The inner surface of the passage of dry-type hollow reactor process for protecting a small space according to Claim 1, characterized in that said step (b) in the device for plugging a rubber air bag, the rubber bag is used for support of the T-shaped copper-iron pipe, first of all the rubber air pocket is placed at the bottom of the reactor air passage, then through the gas distributor to the rubber air bag can be inflated to its expansion, the bottom of the air passage of the plugging of the reactor.

3. The inner surface of the passage of dry-type hollow reactor process for protecting a small space according to Claim 1, characterized in that said step (b) the sealing device of the in the guiding of the pipeline recovery with valve frame-proof plaster, rubber or silicone rubber, the reactor is at the bottom of the channel, exerting a force on the blocking device, air blocking the bottom of the reactor.

4. The inner surface of the passage of dry-type hollow reactor process for protecting a small space according to Claim 1, characterized in that said step (c) in, through the coating material recovery device, the coating material to the coating dispenser, and then respectively the coating through the coating dispenser delivery to the plurality of branch pipe, the jet pipe is in charge of the coating, the dip-coating of the inner surface of the passage of the reactor.

5. The inner surface of the passage of dry-type hollow reactor process for protecting a small space according to Claim 1, characterized in that said step (c) in, the air in the reactor by spraying or pouring the coating means for coating the reactor of perfusion, the dip-coating of the inner surface of the passage of the reactor.

6. The inner surface of the passage of dry-type hollow reactor process for protecting a small space according to Claim 1, characterized in that said step (d) in, when the paint injection or perfusion to the air after the upper edge of, the outdoor temperature at the construction site, the coating in the reactor for the delay time of the air flue 1-30min, the reactor of the coating on the surface of the dip-coating, coating and reactor air passage to fully contact the inner surface to form a protection coating.

7. The inner surface of the passage of dry-type hollow reactor process for protecting a small space according to Claim 1, characterized in that said step (e) in, through the coating material recovery device for the coating of the reactor to the air recovery processing.

8. The inner surface of the passage of dry-type hollow reactor process for protecting a small space according to Claim 7, characterized in that it also comprises the coating of the reactor air passage at the bottom of the reactor oddments recovery device on the air passage of the residual water in the recovery processing.

9. The inner surface of the passage of dry-type hollow reactor process for protecting a small space according to Claim 2, characterized in that said step (f) in, the reactor at the bottom of the air bleed of the rubber bag, then through the T-shaped copper iron pipe to the rubber bag is drawn out from the bottom, the reactor block at the bottom of the completion of the removal of air.

10. The inner surface of the passage of dry-type hollow reactor process for protecting a small space according to Claim 3, characterized in that said step (f) in, the bottom of the reactor for removal of air to the anti-seggar or rubber, the stress of the silicone rubber, the completion of removal of the plugging of the reactor at the bottom of the channel.