23-06-2023 дата публикации
Номер: CN116275412A
Принадлежит:
The invention discloses a welding method of high manganese steel and 9Ni dissimilar steel, which adopts electric arc welding, the welding current is 110-130 A, the arc voltage is 21-24 V, the welding speed is 10-13 cm/min, and the welding heat input is 10-18 kJ/cm; and the interlayer temperature does not exceed 100 DEG C. The welding groove is X-shaped, the angle of the groove is 60-70 degrees, the thickness of the truncated edge of the groove is 0-2 mm, and the gap of the groove is 0-2 mm. According to the method, the impact energy KV2 of a weld joint and a heat affected zone at the temperature of minus 196 DEG C is larger than or equal to 27J, the tensile strength is larger than or equal to 680MPa, the longitudinal face bend d of a welded joint is 4a, the welded joint is qualified at 180 degrees, and the mechanical properties required by various low-temperature environments are met; the process window is proper, operability is high, special equipment and process conditions are not needed ...