27-06-2023 дата публикации
Номер: CN116332517A
Принадлежит:
The invention provides transparent glass ceramic with a low expansion coefficient and a preparation method thereof. The glass ceramic comprises the following components in percentage by mass: 60%-75% of SiO2, 15%-28% of Al2O3, 0.5%-2% of TiO2, 2%-5% of ZrO2, 2%-8% of Li2O, 0%-1% of MgO, 1%-4% of CeO2 + SnO2 + P2O5 + Nd2O3 + ZnO, 0.3%-1.2% of (TiO2 + P2O5 + ZrO2)/Li2O, 0.3%-1.2% of (MgO + ZnO)/(SiO2 + Al2O3) lt, 0%-1% of MgO, 0%-1% of Na2O, 0%-1% of Na2O, 0%-1% of Na2O, 0%-1% of Na2O, 0%-1% of Na2O, 0%- And 0.02 part. Through component design, a stepped nucleation process and accurate crystallization process regulation and control, the high-strength and high-transmittance low-expansion transparent microcrystalline glass is obtained, the linear expansion coefficient of the glass is reduced, and the size of precipitated crystal grains is controlled, so that the microcrystalline glass subjected to heat treatment has excellent mechanical properties, optical properties and chemical stability.