04-08-2023 дата публикации
Номер: CN116535171A
Принадлежит:
The invention discloses a method for preparing concrete from lithium feldspar powder, and belongs to the technical field of concrete.The method comprises the following steps that S1, under the nitrogen protection condition, amino-functionalized zeolite powder, dicarboxyl monomers, pyridine and triphenyl phosphite are added into an N-methyl pyrrolidone solution, stirring reaction is conducted for 3 h at the temperature of 80 DEG C, then dicarboxyl amino acid is added, stirring reaction is conducted for 3 h at the temperature of 80 DEG C, and a mixture is obtained; keeping the temperature unchanged, and continuously reacting for 3-4 hours to obtain grafted modified zeolite; s2, levigating the lithium feldspar powder until the specific surface area is 400-420m < 2 >/kg, mixing the cement, the graft modified zeolite, the lithium feldspar powder, the fine aggregate, the coarse aggregate and water, and curing after a workpiece is manufactured, so as to obtain the concrete. According to the invention ...
Подробнее